Impahla ye-ramming yesithando somlilo esimaphakathi

I-Acid dry ramming material: Ngemva kokomiswa kwesithando somlilo sokuqala kanye ne-sintering α- Phosphorus quartz inezinga eliphezulu lokuguqulwa, isikhathi esifushane sokumisa, ukuqina kwevolumu okuhle kakhulu, ukuzinza kokushaqeka okushisayo namandla okushisa aphezulu.

Imininingwane

Isithando somlilo esimaphakathi
ramming impahla

Impahla ye-ramming ephakathi nendawo
I-ramming eyomile engathathi hlangothi ibonakala ngokusetshenziswa kalula, ukuqina ekushiseni okujwayelekile, amandla okucindezela okushisa aphezulu, ukunwetshwa okuncane kokushisa kanye nokuncipha, nokumelana okuqinile nokuguguleka kwesisombululo.

I-alkaline dry ramming material
I-alkaline dry ramming material inezinzuzo zokuzinza kwevolumu yokushisa okuphezulu, ukumelana nokuguguleka, ukumelana nokugqokwa, ukumelana nokushaqeka okuhle kokushisayo, izinga lokushisa lokuthambisa umthwalo, njll.

Izinkomba zomzimba nezamakhemikhali zemikhiqizo

Ukuma kwempahla

MgO

I-Al2O3

I-CaO

SiO2

Ukuminyana ngobuningi

Usayizi wezinhlayiya

Izinga lokushisa eliphezulu lesevisi

I-Lithic

-

-

-

98

1.9~2.2

0~6

1650

Magnesium

≥96

<1.5

-

<2

2.85~2.9

0~10

1800

I-Al mg spinel

11-32

65-88

1

1

2.95~3.15

0~6

1800

Corundum

-

90

-

-

2.95~3.15

0~6

1800

Mullite

-

>80

-

<16

2.6

0~6

1400

I-Magnesia alumina spinel

75

22

-

-

3.05

0~6

1800

Izinto eziphikisayo ezinezinkomba ezihlukene zingenziwa ngokwezifiso ngokwesidingo. Shayela ku-400-188-3352 ngemininingwane